After the soda blast.... I hand sanded down the entire body.  The interior is removed.  I just finished POR15'ing the floor area and windshield trim.  No damage to fix.  What filler do I use before I prime it to paint?  Thanks.

2 Answers

1,255

You want to use a fiberglass filler from Eckler's, use an epoxy primer to give your body an armor finish that will not crack or more important, not let gases like Freon R11 or 22 to escape and seep into your fiberglass hood. Once it gets into the hood and right front fender, the paint will always look funny. Almost like fisheyes.Then a nice thin base coat, and at least three coats of clear . Pound it down and stand back and be amazed.

2 people found this helpful.
10

Thank you for the insight; I have never thought of the gases seeping into the fiberglass.

1 people found this helpful.

Your Answer:

CarGurus Experts

  • #1
    John Carson
    Reputation
    5,210
  • #2
    Vincent Parker
    Reputation
    4,730
  • #3
    dandyoun
    Reputation
    1,400
View All

Find great deals from top-rated dealers

Search

Related Models For Sale

Used Chevrolet Camaro
22 Great Deals out of 471 listings starting at $11,999
Used Dodge Challenger
24 Great Deals out of 771 listings starting at $11,480
Used Dodge Charger
36 Great Deals out of 865 listings starting at $5,995
Used Porsche 911
19 Great Deals out of 242 listings starting at $22,980
Used Ford F-150
301 Great Deals out of 13,535 listings starting at $3,888
Used BMW 3 Series
62 Great Deals out of 1,164 listings starting at $2,500

Content submitted by Users is not endorsed by CarGurus, does not express the opinions of CarGurus, and should not be considered reviewed, screened, or approved by CarGurus. Please refer to CarGurus Terms of Use. Content will be removed if CarGurus becomes aware that it violates our policies.